MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT ALPA-SIL TD ANTIST. SH. A 12 Silicone Molding Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: Pourable, addition-curing, 2-part silicone rubber that cures at room temperature. This product is mainly used for making antistatic silicone printing pads. The cured rubber exhibits excellent physical and electrical properties. Fast and non-shrink cure at room temperature which can be accelerated considerably by the application of heat.

Key Features

  • Easy 1:1 mix ratio
  • Antistatic properties
  • Pink or green options
  • For use as a printing pad elastomer
Application: Soft Silicone Elastomer with antistatic properties for Pad-Printing applications.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 8000 cPA
 8000 cPB
 8000 cPMixed
Linear Mold Shrinkage <= 0.0010 cm/cm
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 12DIN 53 505
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 12.0 hourTack Free Time / Skin Formation
 12.0 hourDe-mould Time / Full Cure
Pot Life 60.0 - 90.0 min
Shelf Life 12.0 Month
 
Descriptive Properties
AppearancePink or Green
ColorPink or GreenCured Product
 TranslucentA
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL116 / 314599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.