MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Oxygen-free low phosphorus Copper, UNS C10800, H80 (35%) Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: refrigerators, air conditioners, gas and heater lines, oil burner tubes, brewery tubes, condenser and heat exchanger tubes, dairy and distiller tubes, pulp and paper lines, tanks, air, gasoline, hydraulic and oil lines.

Test specimens: rod - 25mm OD.

Key Words: AMAX-LP Copper
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4747
Hardness, Rockwell F 8787
Tensile Strength, Ultimate 330 MPa47900 psi
Tensile Strength, Yield 305 MPa44200 psi
Elongation at Break 16 %16 %in 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Fatigue Strength 115 MPa16700 psi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 185 MPa26800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000187 ohm-cm
@Temperature 20.0 °C
0.00000187 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 350 W/m-K
@Temperature 20.0 °C
2430 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1083 °C<= 1981 °F
Solidus 1083 °C1981 °F
Liquidus 1083 °C1981 °F
Annealing Point >= 482 °C>= 900 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 375 - 650 °C707 - 1200 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %Includes Ag
Phosphorus, P 0.0050 - 0.012 %0.0050 - 0.012 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC10800c3 / 10484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.