MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These superior properties together with excellent drawability make this a versatile polymer for mono layer and multi layer cast stretch film applications.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Artificial grass
  • Cast Film
  • Cast Stretch Film
  • Diaper Backsheet
  • Hygiene Film
  • Overwrap Film
  • Personal Care

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccExxonMobil method
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1500 psiASTM D882
Film Tensile Strength at Yield, TD 1400 psiASTM D882
Film Elongation at Break, MD 530 %ASTM D882
Film Elongation at Break, TD 750 %ASTM D882
Puncture Energy 23.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 70 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test 60.0 gASTM D1709
Film Tensile Strength at Break, MD 8900 psiASTM D882
Film Tensile Strength at Break, TD 5900 psiASTM D882
1% Secant Modulus, MD 27000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 250 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 2.8 %ASTM D1003
Gloss 87 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force10 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications

PEX99039 / 175275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.