MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chambroad Petrochemicals SBRL-1354 Styrene-butadiene Rubber Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: High-solid-content Styrene-butadiene Rubber Latex: I. SBRL-1354 Cationic Styrene-butadiene Rubber Latex SBRL-1354 cationic styrene-butadiene rubber latex, a stable emulsion formed through emulsion polymerization of 1,3-butadiene andstyrene, has good great adhesion, stability, and fluidity.SBRL-1354 is a high-performance, high-solid-content styrene-butadiene rubberlatex for modified emulsified asphalt, and it is synthesized by moderately adjusting the polymerization process according to thecharacteristics of emulsified asphalt for pavement. The introduction of the product into the modified emulsified asphalt can reduce thetemperature sensitivity of the asphalt, increase its ductility and cracking resistance at low temperatures, improve the asphalt'sproperties at high temperatures, including softening points and elasticity, and enhance the adhesion of asphalt and chips. II. SBRL-2263 Anionic Styrene-butadiene Rubber Latex SBRL-2263 is a water-based non-curable styrene-butadiene rubber latex for quick setting by spraying.The product has goodcompatibility with waterproof coating of anionic emulsified asphalt, reconciliation, chemical stability, and mechanical stability, and cansignificantly improve the waterproofness, high-temperature resistance, and low-temperature flexibility of the waterproof coating ofanionic emulsified asphalt, and greatly improve its adhesion, crack resistance, and puncture resistance after coating film formation. Itovercomes the performance of general styrene-butadiene rubber latex modified emulsified asphalt waterproof coating which is notresistant to puncture and poor elastic recovery after curing, and prolongs the service life of buildings.

Information provided by Shandong Chambroad Petrochemicals Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content >= 60 %>= 60 %
pH 3.0 - 7.03.0 - 7.0
Viscosity <= 2000 cP<= 2000 cPApparent
 
Descriptive Properties
AppearanceMilky white emulsion, free of visible coagula and mechanical impurities
Mechanical stability<2.0%
Particle chargeCation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAMB058 / 318600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.