MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ter Hell Plastic Terez® PA 6 7500 TF 20 GF 20 Polyamide 6, 20% PTFE chemically bonded 20% glass fiber reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, PTFE Filled

Material Notes: Description: Medium viscosity PA 6, 20% PTFE chemically bonded and 20% glass fiber reinforced, good flowability, good impact resistance and bright natural color.

Application: For molding parts with increased stiffness and side loading.

Information provided by Ter Hell Plastic GMBH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccISO 1183
Water Absorption 5.7 %ISO 62
Moisture Absorption at Equilibrium 1.5 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 138 MPadry; ISO 527
Tensile Strength 140 MPadry; ISO 527
Tensile Strength, Yield 145 MPadry; ISO 527
Elongation at Break 3.0 %dry; ISO 527
Elongation at Yield 2.0 %dry; ISO 527
Tensile Modulus 6800 MPadry; ISO 527
Charpy Impact Unnotched 80.0 kJ/m²dry; ISO 179
Charpy Impact, Notched 12.0 kJ/m²dry; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75
Vicat Softening Point 215 °CB/50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 240 - 270 °C
Drying Temperature 90.0 °C
Dry Time 5 - 6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled
Techmer ES HiFill FR® PA6 GF13 FR-N IM BK 13% Glass Filled
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated
Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated

PTERH913 / 120651

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.