MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATI Wah Chang Tiadyne™ 3510
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.

Information provided by ATI Wah Chang

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.190 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 250200 g
Tensile Strength, Ultimate 120000 psiBeta Quenched
 160000 psiFully Hardened
Tensile Strength, Yield 50000 psiBeta Quenched
 150000 psiFully Hardened
Elongation at Break 12 %Fully Hardened
 23 %Beta Quenched
Modulus of Elasticity 62.1 GPaBeta Quenched
 71.7 GPaFully Hardened
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.30 µin/in-°F
@Temperature 500 °C
 7.60 µin/in-°F
@Temperature 100 °C
Thermal Conductivity 52.6 BTU-in/hr-ft²-°F
 125.4 BTU-in/hr-ft²-°F
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Niobium, Nb (Columbium, Cb) 10.7 - 11.7 %
O2 0.070 - 0.13 %
Titanium, Ti 52.1455 - 55.23 %
Zirconium, Zr 34 - 36 %
 
Descriptive Properties
Thermal Diffusivity, cm²/sec0.033

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Wah Chang TI-45 Nb
Goodfellow Nickel 70/Titanium 30 Alloy
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy
Goodfellow Titanium 50/Iron 50 Alloy
Titanium Grade 36 55Ti-45Nb

NATIWC21 / 15076

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.