MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Multi-Way Oil HD ISO Grade 220
Categories: Fluid; Lubricant

Material Notes: Multi-Way Oil HD is a circulating oil developed for the lubrication of lathes and heavily loaded machine tool slideways. It is specially formulated to prevent stick-slip problems to ensure good surface finish on the machined part. Multi-Way Oil HD is formulated with a special tackifier additive that allows machine tool carriages to start easily and move smoothly throughout their travel, thus preventing stick-slip problems. This reduces carriage chatter and ensures a smooth finish on the machined part. Its mild extreme-pressure properties prevent scoring of the slideways during carriage travel. The tackifier improves adhesion and prevents the oil from being squeezed off the slideways. It also helps prevent the oil from being washed away by cutting fluids. Additional additives provide protection against rust and corrosion and allow optimum coolant separation. Multi-Way Oil HD, ISO VG 32 and 68, may be used as a combination way oil, hydraulic oil and gear oil in machine tools where the circulating oil is supplied from a central reservoir.

Applications:

  • Horizontal and vertical slideways on machine tools, such as lathes, planers, shapers, drilling machines, milling machines and screw machines
  • Lumber mill saw carriages
  • Pneumatic equipment, such as jackhammers, pavement breakers and rock drills
  • Moderately loaded enclosed industrial gear drives that require an adhesive gear oil with mild extreme-pressure (EP) properties (ISO VG 220)
  • Hydraulic systems operating at less than 1,000 psi (ISO VG 32, 68)
Features/Benefit:
  • Excellent anti-stick-slip performance
  • Good surface finish
  • Protects against scoring and wear
  • Good adhesion for retention on slideways
  • Protects against rust and corrosion
  • Excellent coolant-separating properties

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/cc
Density 7.33 lb/gal
Viscosity Measurement 101Index
Saybolt Viscosity at 100°F 1160 SUS
Saybolt Viscosity at 210°F 99.4 SUS
Kinematic Viscosity at 40°C (104°F) 220 cSt
Kinematic Viscosity at 100°C (212°F) 19.6 cSt
ASTM Color 6.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.35[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °C
Flash Point 260 °CCOC
 
Descriptive Properties
Demulsibility15 minutes to passASTM D1401
Slip0.67Stick-Slip, ASTM D2877

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5191 / 198444

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.