MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sirmax Xelter® S 111A85-xxx-yyy-F TPS (SEBS)
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Applications: Injection Molding

Information provided by Sirmax®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ASTM D729
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85
@Time 3.00 sec
85
@Time 0.000833 hour
ASTM D2240
Tensile Strength 14.0 MPa2030 psiASTM D412-C
Elongation at Break 750 %750 %ASTM D412-C
100% Modulus 3.40 MPa493 psiASTM D412-C
Tear Strength 40.0 kN/m228 pliASTM D624-C
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 195 °C383 °F
Melt Temperature 170 - 190 °C338 - 374 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIRMX319 / 281422

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.