MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Gargoyle Arctic 300
Categories: Fluid; Lubricant

Material Notes: Gargoyle Arctic 155, C Heavy and 300 products are high performance naphthenic mineral oils primarily intended for use in refrigeration compressors. They have low pour points and excellent fluidity at very low temperatures by virtue of being almost wax-free. Consequently, use of these Gargoyle Arctic oils ensures that evaporator tubes are kept clean to improve heat transfer and to reduce downtime for maintenance. They have good chemical stability and are suitable both for cylinder and bearing lubrication. Gargoyle Arctic 155, C Heavy and 300 are compatible with all refrigerants except sulphur dioxide. They are not recommended for use with HFC refrigerants. The moisture content of Gargoyle Arctic 155, C Heavy and 300 oils is very low when the oils are packaged. Every precaution should be taken to keep the oils dry to avoid the formation of ice in expansion valves, and to limit the risks of oil degradation, copper plating, etc.

The Gargoyle Arctic 155, C Heavy and 300 products are recommended for cylinder and bearing lubrication in all conventional refrigeration compressors and for all other machinery operating at sub-zero temperatures. Typical applications include: Large industrial reciprocating and rotary refrigeration compressors; Industrial applications such as food freezing and cold storage plants; Marine refrigeration applications; Used primarily with ammonia refrigerant, but also used with selected halocarbons

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/cc
@Temperature 15.0 °C
ASTM D1298
Kinematic Viscosity at 40°C (104°F) 68 cStASTM D445
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.010mgKOH/g; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -42.0 °CASTM D97
Flash Point 200 °CASTM D92
 
Descriptive Properties
Flocculation Point, R12, DIN 51351, °C-31

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NRI Syntho-Steel™

WEXXON187 / 75612

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.