MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ Flow PP6936G2 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Exceed™ PP6936G2 is an ultra high melt flow rate metallocene based homopolymer resin designed for melt blown nonwoven.  Fabrics with superior barrier properties can be produced at reduced process energy demands.  

Availability:  Latin America, North America.  Features: narrow molecular weight distribution.   Applications: filtration media, medical/ healthcare applications, personal care, industrial applications, melt blown nonwovens .   Appearance:  Natural Color.  Forms: granules.  Processing Method: fiber (spinning) extrusion.

Information provided by ExxonMobil.

Key Words: Achieve™ Advanced PP6936G2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 1550 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Achieve™ Advanced PP0502E1 Polypropylene Homopolymer
Graft Polymer GRAFTABOND™ PPH-MAH 20025 CA Maleic anhydride functioned Homopolymer Polypropylene
Graft Polymer GRAFTABOND™ PPH-MAH 15025 CA Maleic anhydride functioned Homopolymer Polypropylene
ExxonMobil PP3746G Granular Homopolymer
ExxonMobil PP3546G Homopolymer Grade for Ultra-High Melt Flow Rate Nonwoven Applications

PEX98972 / 238353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.