Product Description: A highly clarified random copolymer resin designed for general purpose injection molding applications requiring resistance to build up of static electricity. Availability: North America Features: - Antistatic
- Controlled Rheology
- Ethylene Oxide Sterilizable
- High Clarity
Uses: - Caps
- Closures
- Medical/Healthcare Applications
- Packaging
- Rigid Packaging
Processing Method: Injection MoldingInformation provided by ExxonMobil |