MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Park Aerospace Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stability and superior hole-wall integrity.

Key Features and Benefits:

  • Outstanding Z-axis, thermal stability and hole wall integrity
  • Automotive Testing
  • SI (Signal Integrity) option
  • CAF resistant
  • Cost-effective standard FR-4 processing

Applications/Qualifications:

  • Wireless Handsets
  • Wireless Infrastructure
  • Digital Broadband Multilayers
  • Automotive
  • Underhood Automotive
  • Backplanes
  • Fine-Line Multilayers
  • Fine Pitch BGA Multilayers
  • Direct Chip Attach
  • RoHS Compliant
  • Meets IPC-4101/98 Specifications

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.97 g/cc50% Resin Content; Internal Method
Water Absorption 0.070 %IPC-TM-650.2.6.2.1
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 2800 ksiY; ASTM D3039
 3500 ksiX; ASTM D3039
Poissons Ratio 0.11Y; ASTM D3039
 0.13X; ASTM D3039
Peel Strength 7.50 pliafter solder float; IPC-TM-650.2.4.8
 8.10 pliat elevated temperature; IPC-TM-650.2.4.8.2a
 9.00 pliafter exposure to process solutions; IPC-TM-650.2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmE - 24/125; IPC-TM-650.2.5.17.1
 1.00e+14 ohm-cmC - 96/35/90; IPC-TM-650.2.5.17.1
Surface Resistance 1.00e+13 ohmE - 24/125; IPC-TM-650.2.5.17.1
 1.00e+14 ohmC - 96/35/90; IPC-TM-650.2.5.17.1
Dielectric Constant 3.9
@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
 3.9
@Frequency 1e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
 4.0
@Frequency 1e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
 4.5
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Dielectric Strength 1250 V/milIPC-TM-650.2.5.6.2
Dielectric Breakdown >= 50000 VIPC-TM-650.2.5.6
Dissipation Factor 0.017
@Frequency 2.50e+9 Hz
Stripline; IPC-TM-650.2.5.5.5
 0.017
@Frequency 1e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
 0.018
@Frequency 1e+6 Hz
TFC/LCR Meter; IPC-TM-650.2.5.5.3
Arc Resistance 124 secIPC-TM-650.2.5.1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.67 - 8.33 µin/in-°F
@Temperature -40.0 - 125 °C
X/Y; IPC-TM-650.2.4.41
 27.8 µin/in-°F
@Temperature 50.0 - 155 °C
Z-Axis Alpha 1; IPC-TM-650.2.4.41
 150 µin/in-°F
@Temperature 155 - 260 °C
Z-Axis Alpha 2; IPC-TM-650.2.4.41
Specific Heat Capacity 0.290 BTU/lb-°FASTM E1461
Thermal Conductivity 3.64 BTU-in/hr-ft²-°FASTM E1461
Glass Transition Temp, Tg 150 °CTMA; IPC-TM-650.2.4.24c
 155 °CDSC; IPC-TM-650.2.4.25c
 160 °CDMA (Tan d Peak); IPC-TM-650.2.4.24.3
Decomposition Temperature 330 °C5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0
 
Descriptive Properties
Methylene Chloride Resistance (% Weight Change)0.31IPC-TM-650.2.3.4.3
Pressure CookerPass60 min then solder dip @288ºC until failure (max 10 min.); IPC-TM-650.2.6.16 (modified)
T260 (minutes)16IPC-TM-650.2.4.24.1
Z Axis Expansion (%)3.750ºC to 260ºC; IPC-TM-650.2.4.41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Park Aerospace Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Premix Thermoplastics PREBOARD E1025 Standard Epoxy Circuit Boards
304 Stainless Steel
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness

PPARK112 / 89384

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.