MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ovako 100CrMnSi6-6 832K Steel, Q/T (martensite)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: General Information: Ovako 832 is a through hardening bearing steel that is mainly used for medium sized bearing rings, but can also be used for machine components that require high tensile strength and high hardness.
  • 40 mm maximum wall thickness for through hardening
  • Used for martensitic hardening
  • Can be induction hardened
  • Good machinability in soft annealed condition
  • Machiable in hardened condition using hard-turning techniques (CBN tools)
  • Ovako 832 is weldable if pre-heated, otherwise risk of hot-cracking
  • Very good dimension stability
832K - Bearing quality (BQ) variant

BQ-Steel: (Bearing Quality) is a bearing quality clean steel optimized for fatigue strength by a strict control of steel cleanliness. BQ-steel is also ideal for new design solutions in a wide array of demanding applications outside the bearing industry that require longer performance and higher loads. The BQsteel offer is the result of the Ovako clean steel program. Purity of production means that the material has significantly smaller inclusions compared to conventional steel and, as a result, the fatigue strength of the steel is increased dramatically. Use of the material allows components to be manufactured in smaller sizes. The BQ-steel has for decades been the problem-solver.

Information provided by Ovako

Key Words: 100CrMnSi6-4, ASTM A485 grade 2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 62
@Thickness <=15.0 mm
Tensile Strength 2300 MPa
@Thickness <=15.0 mm
Tensile Strength, Yield >= 1700 MPa
@Thickness <=15.0 mm
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 229 °CMS
 723 °CAC3
 749 °CAC1
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.87 - 0.97 %
Chromium, Cr 1.4 - 1.7 %
Iron, Fe 94.2 - 95.47 %As Balance
Manganese, Mn 1.5 - 1.7 %
Molybdenum, Mo 0.060 - 0.10 %
Nickel, Ni 0.10 - 0.50 %
Phosphorus, P <= 0.015 %
Silicon, Si 0.60 - 0.80 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Ovako 100CrMo7 824B Steel
Ovako 100CrMnSi6-6 832K Steel, Spheroidize annealing
Ovako 100CrMnSi4-4 831B Steel, Spheroidize annealing
Ovako 100CrMnMoSi8-4-6 827B Steel, Spheroidize annealing

NOVAKO043 / 234342

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.