MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss of paper coatings, aid in pigment dispersion and mold release, and improve scuff and rub off resistance in printing inks.
    Key Attributes:
  • Aids in pigment dispersion
  • Easy to melt blend with natural or synthetic waxes
  • Improves physical properties of paper coatings
  • Increases scuff and rub off resistance in inks
  • Low density polyethylene (PE)
    Application/Uses:
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solventborne Adhesives
  • Wax Modification
  • Automotive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 - 0.950 g/cc
Viscosity 550 - 850 cP
@Temperature 125 °C
542-111
Brookfield Viscosity 700 cP
@Temperature 125 °C
Molecular Weight 7580 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 343 °CASTM E136
Ring & Ball Softening Point 104 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.0542-130
 
Descriptive Properties
Penetration Hardness 3 dmmASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWESF9033 / 106870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.