  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Extra High Leaded Brass, UNS C35600, O60 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Soft Anneal

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Butt Weld, Capacity for Being Hot Formed; Poor Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Machining; Piercing and Punching; Stamping

Typical uses: Clock and Watch Backs; Clock Gears and Wheels; Clock Plates and Nuts; Channel Plate

Applicable Specifications: Bar – ASTM B121/B121M; Plate - ASTM B121/B121M; Rod, Bar & Shapes – ASTM B453/B453M; Sheet – ASTM B121/B121M; Strip – ASTM B121/B121M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.307 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 40.0 ksi
@Thickness 34.92 mm
 >= 44.0 ksi
@Thickness 19.0 mm
 >= 46.0 ksi
@Thickness <=12.7 mm
Elongation at Break >= 20 %
@Thickness <=12.7 mm
 >= 25 %
@Thickness 19.0 mm
 >= 30 %
@Thickness 34.92 mm
Tensile Modulus 14000 ksi
Modulus of Rigidity 5300 ksi
Poissons Ratio 0.32Calculated
Machinability 100 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm26% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.4 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 67.0 BTU-in/hr-ft²-°F
Melting Point 1630 - 1660 °F
Solidus 1630 °F
Liquidus 1660 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1300 - 1450 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 60 - 63 %
Iron, Fe <= 0.15 %
Lead, Pb 2.0 - 3.0 %
Zinc, Zn 34 - 38 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC35600x8 / 292942

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.