MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT HANSA CARE 5711 Emulsion of a modified siloxane
Categories: Other Engineering Material

Material Notes: Description: Whenever liquids are moved, pumped or agitated there is a risk of foam being developed. Large amounts of foam will often slow down the production process, inhibit chemical reactions and impair product performance.

Key Features

  • Foam control
  • High shearing stability
  • pH stability in the range of 3 – 13
  • Good dispersability in aqueous systems
Key Applications
  • Floor Care
  • Kitchen and Sanitary Cleaner
  • Cleaner Formulations
Application: HANSA CARE 5711 may be used to prevent or destroy foam in a wide range of acid, neutral and alkaline aqueous systems.

Addition Rates
Dosage – 1: 0.1 – 1.0% in water based formulations

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 85 %85 %
pH 7.0 - 8.07.0 - 8.0
Brookfield Viscosity 1000 - 2500 cP1000 - 2500 cP
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceWhite emulsion
ChemistryEmulsion of a modified siloxane
IonicityNon-ionic
MIT FreeNo
Ultralow cyclic contentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL234 / 314717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.