MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.

Customer Benefits: DK13 is an SBC designed for the film market and has increased tear and higher elongation properties. It has improved processability and a reduced tendency to form wrinkles during the film manufacturing and converting process. Film produced has excellent clarity, high surface gloss, good heat sealability, good toughness, good stiffness, and excellent tear strength. Film shrinkage is 72% MD and 31% TD.

Applications: Major applications include medical packaging, produce packaging, skin packaging, twist wrap, lidstock film, labeling film, decorative films, industrial films, shrink wrap, overwrap film, barrier film, and tamper evident packaging

Processing Recommendations:
Blown Film: Melt temperature between 166-193°C recommended. Cast film: Melt temperature between 193-216°C recommended. High shear and restrictive type screws tend to degrade the melt.

Specification Data: FDA Regulation 21 CFR 177.1640. Suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL 94HB.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Moisture Vapor Transmission 0.300 cc-mm/m²-24hr-atm0.762 cc-mil/100 in²-24hr-atm@ 23°C; ASTM F1249
Oxygen Transmission 100 cc-mm/m²-24hr-atm254 cc-mil/100 in²-24hr-atmASTM D3985
Melt Flow 10 g/10 min10 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 20.0 MPa2900 psi2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 16.0 MPa2320 psi2 in per min; ASTM D882
Film Elongation at Break, MD 207 %207 %ASTM D882
Film Elongation at Break, TD 260 %260 %ASTM D882
Secant Modulus, MD 0.696 GPa101 ksiat 1%; ASTM D882
Secant Modulus, TD 0.469 GPa68.0 ksiat 1%; ASTM D882
Elmendorf Tear Strength, MD 0.175 g/micron4.44 g/milASTM D1922
Elmendorf Tear Strength, TD 0.0760 g/micron1.93 g/milASTM D1922
Dart Drop Test 325 g0.717 lb26 in; ASTM D1709
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003
Gloss 125 %125 %45°; ASTM D2457
Transmission, Visible 94 %94 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 166 - 193 °C331 - 379 °FBlown Film
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR03BR SBC
Chevron Phillips K-Resin® KR01BR SBC
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade

PCHEVK35 / 20280

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.