MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Alliance C-1 Sintered SrO-6Fe2O3 Ferrite Magnet
Categories: Ceramic; Oxide

Material Notes: Ferrite magnets, commonly called ceramic magnets, are the most widely used magnet materials. These are the least expensive permanent magnets and are mostly used in Electric Motors and loud speakers.

Information provided by Alliance LLC.

Key Words: Hard Ferrite Ceramic Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 4.90 g/cc>= 0.177 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 34.5 MPa5000 psi
Modulus of Elasticity 179 GPa26000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1e+05
@Temperature 20.0 °C
1e+05
@Temperature 68.0 °F
Magnetic Coercive Force, Hc 1750 - 2050 Oe1750 - 2050 Oe
 3100 - 3400 Oe3100 - 3400 OeIntrinsic
Magnetic Remanence, Br 2250 - 2450 Gauss2250 - 2450 Gauss
Magnetic Maximum Energy Product, BH 0.90 - 2.0 MGOe0.90 - 2.0 MGOe
Curie Temperature 450 °C842 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C5.56 µin/in-°FPerpendicular to M
 14.0 µm/m-°C7.78 µin/in-°FParallel to M
Maximum Service Temperature, Air <= 350 °C<= 662 °FContinuous
 
Descriptive Properties
Reversible Temperature Coefficients-0.2α Br. %/°C
 0.35β Hcj. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NALLIAN31p / 268369

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.