Description: The permanently cationic charge makes these polymers excellently suited for a use as spray wax or rinse-off wax. Moreover, silicone quats may work as boosters for other substances which can then be distributed more easily on the surface. Key Features - Sheeting effect
- Drying effect
- Improves Gloss and Color depth
- Smoothness
Key Applications- Car Shampoos
- Polishes
- Cleaners
Application: HANSA CARE 2229 is an additive for shampoos, cleaners and polishes to improve the sheeting effect by rinsing with water. Besides this hydrophobic effect, the silicone leaves a smart shine and deep color after drying. The product may improve the surface smoothness and slip.Addition Rates Dosage - 1 0.3 – 5.0% in shampoos and cleaners Dosage - 2 0.5 – 8.0 % in conditioner preparations INCI Name: Silicone quaternium-29 (and) cocoamide DEA (and) citric acid Information provided by CHT Group |