MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vycom FLAMETEC™ KYTEC® PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical, and ultraviolet environments. Kytec has a continuous use temperature of 235º F. Kytec is chemically resistant to most acids, bases, and organic solvents and is ideally suited for handling wet or dry chlorine, bromine and other halogens.

FEATURES AND BENEFITS

  • Weldability- Easy to fabricate and thermoplastically weldable.
  • Strength- Good tensile strength and mechanical abrasion resistance.
  • Purity- An ultra-pure material.
  • Chemical Resistance- Resistance to a broad range of chemistries.
  • Fire Safe- Meets FM4910 criteria and is FM listed.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 - 1.79 g/ccASTM D792
Water Absorption 0.020 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76 - 80ASTM D2240
Tensile Strength, Ultimate 6000 psiASTM D638
Tensile Strength, Yield 6500 psiASTM D638
Elongation at Break 50 - 250 %ASTM D638
Elongation at Yield 10 %ASTM D638
Tensile Modulus 225000 psiASTM D638
Flexural Strength 6960 - 8000 psiASTM D790
Flexural Modulus 250000 psiASTM D790
Compressive Strength >= 8850 psiASTM D695
Izod Impact, Unnotched 1.50 - 2.50 ft-lb/inASTM D256
Coefficient of Friction 0.10 - 0.25ASTM D1894
Coefficient of Friction, Static 0.15 - 0.25ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.40e+15 ohm-cmASTM D257
Dielectric Constant 6.0
@Frequency 1e+6 Hz
ASTM D150
 6.8
@Frequency 60 Hz
ASTM D150
 6.9
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 12.2 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.013
@Frequency 1000 Hz
ASTM D150
 0.032
@Frequency 60 Hz
ASTM D150
 0.153
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 50 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 56.0 - 67.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.190 - 0.220 W/m-KASTM C177
Maximum Service Temperature, Air 235 °F
Deflection Temperature at 0.46 MPa (66 psi) 257 - 284 °F
Deflection Temperature at 1.8 MPa (264 psi) 221 - 240 °F
Brittleness Temperature -46.0 °FASTM D2236
Oxygen Index 43 %ASTM D2863
 
Descriptive Properties
Factory Mutual4910 ListedFile #3D1Q5.AM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
Omnia Plastica Kynar® PVDF
3M Dyneon™ PVDF 2066_0002 Fluoroplastic
Adamas Lakinor® U PVDF
CENTROPLAST CENTROFLON Polyvinylidene fluoride

PCPCV07 / 29079

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.