MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Nylene® Nylene 5150 HS Nylon 66, 50% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: 50% glass fiber reinforced, heat-stabilized nylon 6/6 injection molding resin. Formulated to exhibit maximum stiffness for the most demanding applications. Should be used in parts and tools specifically designed to accommodate such high glass fiber loadings, in order to maximize part performance.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.56 g/ccASTM D792
Linear Mold Shrinkage 0.0020 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 193 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Modulus 10070 MPaASTM D790
Izod Impact, Notched 160 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 254 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 249 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Esstech X-951-0050 BisGMA/Triethyleneglycol Dimethacrylate (50/50)
Nylene® PA6/6 Glass Filled 5150 HS Nylon 6/6
Lord Adhesives Chemlok® 5150 Adhesive
Ipiranga Petrochem GF 5150 HDPE
Ipiranga Petrochem GD 5150 K HDPE

PNYLEN967 / 221499

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.