MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC MX2 High Wear Fine Particle Wear Compound
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”) or more. Non-Shrinking, 100% solids. ARC MX2 is formulated with a high concentration of ceramic beads and fine ceramic particles for extremely abrasive environments where metal loss is often repaired by more conventional and costly weld overlay. ARC MX2 is a long lasting wear resistant surface which frequently outperforms the original metal, rubber liners, ceramic tiles or weld overlay. ARC MX2 is a long lasting wear resistant surface and is chosen over the ARC Composites where risk of dark contamination is critical.

Benefits:

  • Excellent wear characteristics of ARC MX2 extend equipment operating cycles.
  • Tough resin structures resist thermal-mechanical shock
  • Outstanding adhesion results in reliable performance with no undercutting
  • Ease of application reduces labor and downtime costs
  • It can be easily shaped and formed to any metal surface.

Suggested Uses:

  • Cyclones
  • Hydrosparators
  • Hopper Bins
  • Pulp Dewatering Screws
  • Wear Plates
  • Porcelain manufacturing equipment
  • Stock Pumps
  • Ball Mills
  • Cleaner Cones
  • Pipe Elbows
  • Pulverizers.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.40 g/cc0.0867 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105
Hardness, Shore D 9090ASTM D2240
Tensile Strength at Break 28.3 MPa4100 psiASTM D638
Flexural Strength 51.7 MPa7500 psiASTM D790
Compressive Strength 90.3 MPa13100 psiASTM D695
Impact Test 7.91 J5.83 ft-lbReverse; ASTM D2794
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 95.0 °C203 °FWet Service
 205 °C401 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  90.0 min
@Temperature 43.0 °C
1.50 hour
@Temperature 109 °F
Light Load
 360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
Light Load
 480 min
@Temperature 25.0 °C
8.00 hour
@Temperature 77.0 °F
Light Load
 720 min
@Temperature 43.0 °C
12.0 hour
@Temperature 109 °F
Full Load
 1200 min
@Temperature 32.0 °C
20.0 hour
@Temperature 89.6 °F
Full Load
 1440 min
@Temperature 16.0 °C
24.0 hour
@Temperature 60.8 °F
Light Load
 1440 min
@Temperature 43.0 °C
24.0 hour
@Temperature 109 °F
Full Chemical
 1800 min
@Temperature 32.0 °C
30.0 hour
@Temperature 89.6 °F
Full Chemical
 2160 min
@Temperature 10.0 °C
36.0 hour
@Temperature 50.0 °F
Light Load
 2160 min
@Temperature 25.0 °C
36.0 hour
@Temperature 77.0 °F
Full Load
 2880 min
@Temperature 16.0 °C
48.0 hour
@Temperature 60.8 °F
Full Load
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Full Chemical
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
Full Load
 4320 min
@Temperature 16.0 °C
72.0 hour
@Temperature 60.8 °F
Full Chemical
 5760 min
@Temperature 10.0 °C
96.0 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  19.8 min
@Temperature 43.0 °C
0.330 hour
@Temperature 109 °F
 120 min
@Temperature 32.0 °C
2.00 hour
@Temperature 89.6 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
 420 min
@Temperature 16.0 °C
7.00 hour
@Temperature 60.8 °F
 960 min
@Temperature 10.0 °C
16.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS027 / 138139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.