Moplen RP3386 is a polypropylene random copolymer used for extrusion applications. Moplen RP3386 has a very narrow molecular weight distribution and is formulated with an anti-gas fading stabilization package. Moplen RP3386 is used for the production of textile filaments with remarkably high softness. Typical application is spun bonded nonwovens. Applications: Filament Yarn, Hygiene Nonwoven, Nonwovens, Wipes/Tissues.Information provided by LyondellBasell. |