MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Crucible Steel 422 Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is capable of being heat treated to various high strength levels depending on section, form, and application involved. Crucible 422 offers designers in the aircraft and power industries high strength/weight ratios from room temperature to 1200°F. The composition is carefully balanced to provide a microstructure which is virtually all tempered martensite after heat treatment. This structure assures uniformity of mechanical properties with a minimum of directionality.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.78 g/cc7.78 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3535Double tempered; Tempering Temperature- 1350°F
 4848Tempering Temperature- 700°F
Tensile Strength, Ultimate 1030 MPa149000 psiTempering Temperature- 1200°C
 1580 MPa229000 psiTempering Temperature- 600°F
 393 MPa
@Temperature 649 °C
57000 psi
@Temperature 1200 °F
Tempering Temperature-1200°F
 1590 MPa
@Temperature 316 °C
230000 psi
@Temperature 600 °F
Tempering Temperature-800°F
Tensile Strength, Yield  317 MPa
@Temperature 649 °C
46000 psi
@Temperature 1200 °F
Tempering Temperature-1200°F
 1050 MPa
@Temperature 316 °C
153000 psi
@Temperature 600 °F
Tempering Temperature-800°F
 862 MPa
@Strain 0.2 %
125000 psi
@Strain 0.2 %
Tempering Temperature-1200°F
 1000 MPa
@Strain 0.2 %
145000 psi
@Strain 0.2 %
Tempering Temperature- 600°F
Elongation at Break 16 %16 %in 2"; Tempering Temperature- 600°F
 19 %19 %in 2"; Tempering Temperature- 1200°F
 16 %
@Temperature 316 °C
16 %
@Temperature 600 °F
Tempering Temperature-800°F
 21 %
@Temperature 649 °C
21 %
@Temperature 1200 °F
Tempering Temperature-1200°F
Reduction of Area 52 %52 %Tempering Temperature-1200°F
 56 %56 %Tempering Temperature- 600°F
 13 %
@Temperature 316 °C
13 %
@Temperature 600 °F
Tempering Temperature-800°F
 85 %
@Temperature 649 °C
85 %
@Temperature 1200 °F
Tempering Temperature-1200°F
Modulus of Elasticity 205 GPa29800 ksi
 141 GPa
@Temperature 593 °C
20500 ksi
@Temperature 1100 °F
Poissons Ratio 0.230.23
 0.16
@Temperature 593 °C
0.16
@Temperature 1100 °F
Shear Modulus 62.1 GPa9000 ksi
 82.7 GPa
@Temperature 23.9 °C
12000 ksi
@Temperature 75.0 °F
Charpy Impact 8.13 - 9.49 J6.00 - 7.00 ft-lbRT
 4.07 - 5.42 J
@Temperature -73.3 °C
3.00 - 4.00 ft-lb
@Temperature -100 °F
 43.4 - 51.5 J
@Temperature 204 °C
32.0 - 38.0 ft-lb
@Temperature 400 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.6 µm/m-°C
@Temperature 21.1 - 260 °C
5.90 µin/in-°F
@Temperature 70.0 - 500 °F
 12.1 µm/m-°C
@Temperature 21.1 - 649 °C
6.70 µin/in-°F
@Temperature 70.0 - 1200 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 25.1 W/m-K
@Temperature 100 °C
174 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.23 %0.23 %
Chromium, Cr 11.5 %11.5 %
Iron, Fe >= 84.12 %>= 84.12 %As Remainder
Manganese, Mn 0.75 %0.75 %
Molybdenum, Mo 1.0 %1.0 %
Nickel, Ni 0.80 %0.80 %
Silicon, Si 0.35 %0.35 %
Tungsten, W 1.0 %1.0 %
Vanadium, V 0.25 %0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 420 Martensitic Stainless steel
AK Steel 439 Ferritic Stainless steel
Crucible Steel 431 Chromium Steel
420 Stainless Steel
ATI Allvac® Vasco® 422 Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal

NCRUC044 / 16037

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.