MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hoskins Manufacturing Chromel® Thermocouple Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usage

Chromel® is a registered trade name of Hoskins Manufacturing.

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM E230
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.3154 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95000 psiAnnealed
 145000 psiStress relieved
 150000 psiHard
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 425 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.1 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.448 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 19.2 W/m-K
Melting Point 2606 °F
Maximum Service Temperature, Air 1260 °COperating Temperature
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 10 %
Nickel, Ni 90 %
 
Descriptive Properties
MagneticNone
Temperature Coefficient of Resistance0.00032 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Goodfellow T1-Thermocouple Alloy
Tophel® Type E Thermocouple Alloy

NHOS2 / 17352

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.