MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Geniosil® CS2 Silane Preparation
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Properties: GENIOSIL® CS 2, when used as a component of organic/inorganic composites, improves the adhesion between the organic polymer and the inorganic fillers used. This imparts significantly improved flexural strength and impact strength to the composites. It also reduces water absorption and dirt pick-up significantly. GENIOSIL® CS 2 also liberates about 50 % less methanol than conventional adhesion promoters.

Special features: GENIOSIL® CS 2 is an unsaturated alkoxysilane. It´s a clear, colorless liquid with a characteristically aromatic odor. It hydrolyzes in the presence of moisture under liberation of alcohol to form silanols, which can then react with themselves to form siloxanes. Having both silyl and unsaturated organic groups, GENIOSIL® CS 2 is able to function as a molecular bridge between organic and inorganic substrates.

Application: GENIOSIL® CS 2 is principally used in the production of unsaturated polyester resin or polyacrylate composites to increase mechanical strength. GENIOSIL® CS 2 acts as a coupling agent by forming a chemical bridge between the organic resin and the inorganic fillers or pigments used, e.g. quartz, granite or even glass.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.985 g/cc
@Pressure 0.1013 MPa
0.0356 lb/in³
@Pressure 14.69 psi
DIN 51757
Kinematic Viscosity 1.29 cSt1.29 cStDIN 51562
 
Thermal PropertiesMetricEnglishComments
Boiling Point 163 °C
@Pressure 0.1013 MPa
325 °F
@Pressure 14.69 psi
DU-GL A2
Flash Point 50.0 °C122 °FDIN 51755
Ignition Temperature 255 °C491 °Fliquids; DIN 51794

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9307 / 204836

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.