An unreinforced polyamide 6, nucleated and lubricated for injection molding. Eplamid 6 NC HV A2,9 offers all primary properties of unreinforced polyamide 6 with High Viscosity and Production of Films and Monofilaments.Information provided by Epsan Plastik |