MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BYK ADD-VANCE® UV 51 20% active PP based anti-UV masterbatch  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Fields of application: Foils, films, fibers, extruded and injection molded articles made from PP compatible resins, like PP, PP/EDPM, PP/PE/EDPM blends (TPOs).
Examples: Tapes, ropes, carpets, non-wovens, films, fibers, garden furniture, automotive bumpers.

Mode of action and advantages: ADD-VANCE UV 51 provides excellent UV stability to thick PP products and articles with a high surface area like films, fibers and tapes. The HALS stabilizer present in ADD-VANCE UV 51 inhibits the light induced degradation of the substrate. The HALS stabilizer acts as radical scavenger, hydroperoxide decomposer or as quencher.

Advantages: Highly effective light stabilization system for PP products; Very narrow additive content specification for reliable and constant anti-UV performance; To be used in thick (injection molding) and thin-walled articles (tapes, films) and fibers; Long lasting anti-UV protection; High resistance to extraction and low volatility; and Safe handling, dust free

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.525 - 0.650 g/cc
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 290 °C
 
Descriptive Properties
AppearanceWhite to off-white granules
Dosing Level1.0-4.0%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® ABS 8004 UV
Techmer ES HiFill FR® ABS FR UV BK
Techmer ES HiFill FR® ABS FR UV
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Polykemi AB POLYabs S00 AS UV ABS, High Flow, UV-Stabilized, Antistatic

PPADDC33 / 133246

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.