Moplen HP3098 is a polypropylene homopolymer used for extrusion applications. Moplen HP3098 has a ultra-high melt flow rate, a very narrow molecular weight distribution and is in pelletized form. Moplen HP3098 is produced using a non-phthalate Ziegler/Natta catalyst and is used for the production of melt blown nonwovens with outstanding barrier/filtration properties. Moplen HP3098 is also used for compounding applications. Applications: Absorption & Filtration, Hygiene Nonwoven, Nonwovens, Wipes/TissuesInformation provided by LyondellBasell. |