Varcum 29341 is a nitrile modified, two-step powdered phenolic resin. APPLICATION: Formulations designed to attain a soft polishing action similar to that achieved with rubber-bonded grinding wheels. FEATURES: Medium flow, medium cure and coarse grind properties. Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |