MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and flexible in order to resist PCB drop testing.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccPart B
 4.03 g/cc4.03 g/ccPart A
Particle Size <= 20 µm<= 20 µm
Viscosity 13000 - 18000 cP
@Temperature 23.0 °C
13000 - 18000 cP
@Temperature 73.4 °F
20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7777
Tensile Modulus 1.38 GPa201 ksiStorage
Shear Strength 9.598 MPa1392 psiLap
 >= 11.7 MPa>= 1700 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.00020 ohm-cm<= 0.00020 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FBelow Tg
 212 µm/m-°C118 µin/in-°FAbove Tg
Thermal Conductivity 2.30 W/m-K16.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 20.0 °C>= 68.0 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 363 °C685 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
 120 min
@Temperature 125 °C
2.00 hour
@Temperature 257 °F
Pot Life 600 min600 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorAmberPart B
 SilverPart A
ConsistencySmooth thixotropic paste
Mix Ratio by Weight10:2.5
Number of ComponentsTwo
Thixotropic Index4.8
Weight Loss0.26%200°C
 0.56%250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® E3001-6 Electrically Conductive, Silver Epoxy

PPOXYT019 / 141057

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.