MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied by trowel or plastic applicator tool in one or two coats, as required. ARC HT-T is applied at a normal thickness of 900-1150 microns (35-45 mils). It is a 100% solids non-shrinking composite. ARC HT-T provides exceptional corrosion and erosion protection to high temperature equipment handling water solutions. The cured product also provides outstanding blister and abrasion resistance with a high gloss finish

Benefits:

  • Exceptional permeating and blister resistance in high temperature water applications, including mild acids and bases.
  • High gloss surface reduces drag, improves flow and pump efficiency
  • Tough resin structure resist thermal-mechanical shock
  • Outstanding adhesion insures reliable performance with no undercutting or underfilm corrosion
  • Advanced reinforcement design provides outstanding abrasion resistance
  • Ability to in-service cure in static conditions reduces application costs and downtime
  • High voltage spark testable per NACE SP0188

Suggested Uses:

  • Condensers
  • Heat Exchangers
  • Pump Volutes
  • Pump Impellers
  • Condensate Pumps
  • Tanks
  • Valves
  • Pressure Vessels
  • Hot Water Pumps
  • Drill Mud Circulating Equipment
  • Oil/Water Separators
  • Oil Extraction Manifolds
  • Condensate Tanks
  • Evaporators
  • Sugar Process Equipment

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.22 g/cc0.0802 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D2240
Elongation at Break 3.6 %3.6 %ASTM D638
Flexural Strength 53.8 MPa7800 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Compressive Strength 93.1 MPa13500 psiASTM D695
Adhesive Bond Strength 32.8 MPa4760 psiASTM D4541
Impact Test 4.52 J3.33 ft-lbreverse; ASTM D2794
 9.04 J6.67 ft-lbdirect; ASTM D2794
 
Thermal PropertiesMetricEnglishComments
CTE, linear  30.2 µm/m-°C
@Temperature -5.00 - 25.0 °C
16.8 µin/in-°F
@Temperature 23.0 - 77.0 °F
ASTM E228
 90.2 µm/m-°C
@Temperature 125 - 150 °C
50.1 µin/in-°F
@Temperature 257 - 302 °F
ASTM E228
Maximum Service Temperature, Air 110 °C230 °FWet Service
 150 °C302 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 32.0 °C
3.00 hour
@Temperature 89.6 °F
Overcoat Begin
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
Overcoat Begin
 360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
Light Load
 480 min
@Temperature 16.0 °C
8.00 hour
@Temperature 60.8 °F
Overcoat Begin
 540 min
@Temperature 25.0 °C
9.00 hour
@Temperature 77.0 °F
Light Load
 1080 min
@Temperature 16.0 °C
18.0 hour
@Temperature 60.8 °F
Light Load
 2160 min
@Temperature 32.0 °C
36.0 hour
@Temperature 89.6 °F
Service
 2400 min
@Temperature 32.0 °C
40.0 hour
@Temperature 89.6 °F
Overcoat End
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Service
 3120 min
@Temperature 25.0 °C
52.0 hour
@Temperature 77.0 °F
Overcoat End
 4320 min
@Temperature 16.0 °C
72.0 hour
@Temperature 60.8 °F
Overcoat End
 5040 min
@Temperature 16.0 °C
84.0 hour
@Temperature 60.8 °F
Service
Tack-Free Time  180 min
@Temperature 32.0 °C
3.00 hour
@Temperature 89.6 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
 480 min
@Temperature 16.0 °C
8.00 hour
@Temperature 60.8 °F
 
Descriptive Properties
ColorBlack
 Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS041 / 138153

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.