MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyplastics TOPAS® 6013L-17 COC
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Used in optical lenses.

TOPAS is an amorphous copolymer based on the polymerization of ethylene and nor-bornene using metallocene catalysts. Its property profile can be varied over a wide range by adjusting the chemical structure during polymerization.

Information provided by Polyplastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 0.010 %ISO 62
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 63.0 MPa5 mm/min; ISO 527-2/1A
Elongation at Break 2.8 %5mm/min; ISO 527-2/1A
Tensile Modulus 2900 MPa1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 15.0 kJ/m²ISO 179 / 1eU
Charpy Impact, Notched 2.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO-75-1.2
Glass Transition Temp, Tg 140 °C10°C/min; ISO 11357-1,-2,-3
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53ISO 489
Transmission, Visible 91 %
@Thickness 2.00 mm
ISO 13468-1
 
Processing PropertiesOriginal ValueComments
Mold Temperature 80.0 - 120 °C
Injection Velocity 20.0 - 100 mm/sec
Injection Pressure 40.0 - 120 MPa
Back Pressure 5.00 - 15.0 MPa
 
Descriptive Properties
ISO Marking Code>COC<ISO 11469; JIS K6999
Product TypeOptical
UL Yellow Card FileE177491

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007F-600 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013EC-01 COC

PPOLPL126e / 191496

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.