MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PTFE HP 108 PTFE + glass fibre + metal oxide
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Low coefficient of friction and very high wear resistance, increased compressive strength, suitable for universal use in non-lubricated bearings with tempered mating partners, good electrical insulation properties Caution: Higher wear in damp environments than PTFE HP 102.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.28 g/ccDIN EN ISO 1183-1
Deformation >= 7.0 %
@Pressure 13.7 MPa,
Time 86400 sec
ASTM D 621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 55DIN EN ISO 868
Ball Indentation Hardness >= 28.0 MPaDIN ISO 2039-1
Tensile Strength, Yield >= 10.0 MPaDIN EN ISO 527
Elongation at Break >= 125 %50 mm/min; DIN EN ISO 527
Compressive Strength >= 8.00 MPa
@Strain 1 %
ASTM D 695
Coefficient of Friction 0.15 - 0.28pv = 0.7 N/mm2 · m/s; ASTM D3702
Coefficient of Friction, Static 0.080 - 0.20ASTM D3702
K Factor (Wear Factor) 0.010 - 0.020pv = 0.7 N/mm2 · m/s; ASTM D3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 150 µm/m-°C
@Temperature 23.0 - 95.0 °C
ASTM D 696
Melting Point 327 °C
Maximum Service Temperature, Air 280 °Clong term
Minimum Service Temperature, Air -260 °C
 
Descriptive Properties
Colordark red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP083 / 250581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.