MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP190 Synthetic Fabric  (discontinued **)
Categories: Polymer; Thermoset; Aramid; Phenolic

Material Notes: Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications include wear plates for conveyor systems, and compressor and pump vanes.

Thickness Tested: 0.125", 0.250" & 0.500"

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93 - 113
@Thickness 1.57 mm
Flexural Strength 49500 psi
@Thickness 1.57 mm
CW
 66800 psi
@Thickness 1.57 mm
LW
Compressive Strength 75000 psi
@Thickness 12.7 mm
Flatwise
Shear Strength 26000 psi
@Thickness 1.57 mm
Perpendicular
Izod Impact, Unnotched 18.5 ft-lb/in
@Thickness 12.7 mm
CW, E-48/50
 20.0 ft-lb/in
@Thickness 12.7 mm
LW, E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.19
@Thickness 1.57 mm
Cond D-24/23
Dielectric Strength 242 V/mil
@Thickness 1.57 mm
D-48/50
 540 V/mil
@Thickness 1.57 mm
Condition - A
Dielectric Breakdown 9000 V
@Thickness 1.57 mm
D-48/50
 75000 V
@Thickness 1.57 mm
Condition A
Dissipation Factor 0.0461
@Thickness 1.57 mm
Cond D-24/23
Arc Resistance 182 sec
@Thickness 3.17 mm
ASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Flammability, UL94 V-0
 
Descriptive Properties
Bond Strength1,800 lb0.5"

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Cobalt, Co
Rogers Arlon CLTE Microwave Printed Circuit Board Substrate
Park Aerospace Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg

PNORPN561 / 48146

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.