MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Semicosil® 986/1K Silicone Adhesive
Categories: Polymer; Thermoset; Silicone

Material Notes: SEMICOSIL® 986/1K is a non-slump, thermally curable, addition curing one-part silicone rubber.

Special features:

  • ready-to-use, one-part system
  • thixotropic
  • translucent
  • medium hardness
  • high flexibility (low-stress-adhesive)
  • primerless adhesion to many substrates
  • rapid heat cure
  • ultraviolet fluorescing
Application:
  • general purpose adhesive for the electronics industry
  • FIPG and CIPG applications

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³cured
 1.07 g/cc0.0387 lb/in³uncured
Viscosity  35000 cP
@Shear Rate 25.0 1/s
35000 cP
@Shear Rate 25.0 1/s
cured; ISO 3219
 300000 cP
@Shear Rate 0.500 1/s
300000 cP
@Shear Rate 0.500 1/s
uncured; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5151ISO 868
Tensile Strength at Break 5.00 MPa725 psiISO 37
Elongation at Break 200 %200 %ISO 37
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ISO 37
Tear Strength 8.00 kN/m45.6 pliASTM D624B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 93
Dielectric Strength 23.0 kV/mm584 kV/inIEC 243
Comparative Tracking Index >= 600 V>= 600 VDIN IEC 112
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Treatment Temp. 150 °C
0.167 hour
@Treatment Temp. 302 °F
10 mm
 30.0 min
@Treatment Temp. 150 °C
0.500 hour
@Treatment Temp. 302 °F
in a circuatling air oven
 360 min
@Treatment Temp. 100 °C
6.00 hour
@Treatment Temp. 212 °F
10 mm
 
Descriptive Properties
Colortranslucentcured
 translucentuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9426 / 204955

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.