MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals Arcel 310 LV 65% PS/35% PE Interpolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes:

Applications: Resilient/reusable packaging, Sports items, Dunnage

Expansion: Minimum Density Potential (pcf): Single pass continuous - 2.1; Double Pass continuous - 1.5; Batch expansion - 1.6
Prepuff Flow Characteristics: Freshly expanded low density Arcel is sensitive to thermal and mechanical shock. Care must be taken to prevent particle densification.
Expected Federates (pph): Singe pass continuous - 400-600; Double pass continuous- 400-600; Batch expansion - 400-600

Bead Size: Spherized pellet 2X A Size

Molding: Part/tooling design and fill gun placement that accommodate the large particles should be priorities. Cycles: Typically 1 1/2 times an EPS cycle at equivalent density. Steaming cycle is longer than EPS but similar pressure.

Arcel is shipped refrigerated and should remain below 40°F until processed.

Information provided by NOVA Chemicals.

Arcel 310 has been discontinued. Arcel 730 is the replacement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.0240 g/cc>= 0.000868 lb/in³After expansion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVA195 / 55096

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.