MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton ARC NVE VC Vinyl Ester Sealer
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Description: ARC NVE VC (Veil Coat) is a two-component, modified epoxy novolac vinyl ester sealer coat formulated for application by brush, roller or spray at 0.15-0.25 mm (0.07-0.010”) wet film thickness. It is used either to seal the NVE TC (Top Coat) or as a stand alone thin film chemical resistant barrier for concrete in chemical immersion applications.

Benefits:

  • User friendly consistency makes installation and finishing fast and easy.
  • Seals surface for ease of cleaning

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccCured
Volatile Organic Compounds (VOC) Content 70 g/lEPA 24
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength >= 551 psiASTM D4541
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °CWet
 200 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 26.0 °C
Foot Traffic
 1.00 hour
@Temperature 26.0 °C
Light Load
 1.00 hour
@Temperature 26.0 °C
Full Load
 1.50 hour
@Temperature 21.0 °C
Foot Traffic
 1.50 hour
@Temperature 21.0 °C
Light Load
 2.00 hour
@Temperature 21.0 °C
Full Load
 2.50 hour
@Temperature 16.0 °C
Foot Traffic
 3.00 hour
@Temperature 16.0 °C
Light Load
 4.00 hour
@Temperature 10.0 °C
Foot Traffic
 4.00 hour
@Temperature 16.0 °C
Full Load
 6.00 hour
@Temperature 10.0 °C
Light Load
 8.00 hour
@Temperature 10.0 °C
Full Load
 16.0 hour
@Temperature 26.0 °C
Full Chemical
 24.0 hour
@Temperature 21.0 °C
Full Chemical
 28.0 hour
@Temperature 16.0 °C
Full Chemical
 32.0 hour
@Temperature 10.0 °C
Full Chemical
 
Descriptive Properties
ColorGray
 Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties)
Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC

PPTCHS016 / 138128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.