MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polymer Resources PC-FR-IM1 Polycarbonate, Low Temperature Impact and Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Process: Molding or Extrusion
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 5.0 - 10 g/10 min5.0 - 10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.8 MPa7800 psiASTM D638
Tensile Strength, Yield 53.8 MPa7800 psiASTM D638
Flexural Strength 75.8 MPa11000 psiASTM D790
Flexural Modulus 2.00 GPa290 ksiASTM D790
Izod Impact, Notched 7.47 J/cm14.0 ft-lb/inASTM D256
 6.41 J/cm
@Temperature -40.0 °C
12.0 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Gardner Impact >= 36.2 J>= 26.7 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C265 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FASTM D648
Flammability, UL94 V-1
@Thickness 3.17 mm
V-1
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 271 - 293 °C520 - 560 °F
Middle Barrel Temperature 282 - 304 °C540 - 580 °F
Front Barrel Temperature 293 - 316 °C560 - 600 °F
Melt Temperature 282 - 316 °C540 - 600 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 118 - 124 °C245 - 255 °F
Dry Time 3 - 4 hour3 - 4 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kotec Carbotex KFR-30T12 Polycarbonate, Flame Retardant
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
Overview of materials for Polycarbonate, Optical Grade
Lotte Advanced Materials Infino® EN-1052 PC, FR

PPOLYR082 / 57244

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.