Syncure™ S100BL system is a three part moisture crosslinkable compound. S100BL is a UL bullentinized sunlight resistant, low density, black cable insulation compound. Available in a RoHS compliant version. NOTE: Typical Properties measured on 14 AWG with 30 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap. Information provided by PolyOne |