MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.2 %1.2 %50% RH; ISO 62
Water Absorption at Saturation 4.7 %4.7 %ISO 62
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122
Tensile Strength, Yield 210 MPa30500 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Tensile Modulus 11.7 GPa1700 ksiISO 527
Flexural Strength 330 MPa47900 psiISO 178
Flexural Modulus 11.6 GPa1680 ksiISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 11.0 J/cm²
@Temperature -30.0 °C
52.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 90.0 kV/mm2290 kV/inIEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 11357
Maximum Service Temperature, Air 120 °C248 °FContinuous use
 240 °C464 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 40 1 natural (2381) PA 6.6 Dry, 40% Glass Filled, Heat Stabilized
Polyram PlusTek PA340S8 Nylon 6.6 for Injection Molding, 40% Glass-beads Reinforced

PPOLYR832 / 126631

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.