MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Tritan™ Renew VX351HF-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Tritan™ Renew VX351HF-50 is an amorphous copolyester with excellent clarity and impact resistance. The outstanding chemical resistance, hydrolytic stability, and ease of processing make Tritan Renew VX351HF-50 an ideal candidate for a broad spectrum of optical applications such as sunglass lenses, optical glass lenses and safety eyewear. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Eyeglass frames
  • Eyewear
Key Attributes
  • Ease of processing
  • Excellent clarity
  • Excellent hydrolytic stability
  • Outstanding impact resistance
  • Quick cycle times
  • Superior chemical resistance

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Tensile Strength at Break 52.0 MPaASTM D638
 53.0 MPaISO 527
Tensile Strength, Yield 43.0 MPaASTM D638
 43.0 MPaISO 527
Elongation at Break 160 %ISO 527
 210 %ASTM D638
Elongation at Yield 6.00 %ISO 527
 7.00 %ASTM D638
Tensile Modulus 1575 MPaASTM D638
 1620 MPaISO 527
Flexural Yield Strength 62.0 MPaISO 527
 64.0 MPaASTM D638
Flexural Modulus 1575 MPaASTM D638
 1590 MPaISO 527
Izod Impact, Notched 110 J/m
@Temperature -40.0 °C
ASTM D256
 860 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -40.0 °C
ISO 180
 85.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Puncture Energy 53.0 J
@Temperature 23.0 °C
@ Max. Load; ASTM D3763
 57.0 J
@Temperature -40.0 °C
@ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5651ASTM C1648
Abbe Number 31.07ASTM C1648
Haze <= 0.400 %ASTM D1003
Transmission, Visible 91.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 282 °C
Mold Temperature 38.0 - 66.0 °C
Drying Temperature 88.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4229 / 323852

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.