MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mockernut True Hickory Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Carya Tomentosa; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.640 g/cc0.640 g/ccGreen, based on volume
 0.720 g/cc0.720 g/cc12% moisture content, based on volume
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 10.8 GPa1570 ksiGreen
 15.3 GPa2220 ksi12% moisture content
Modulus of Rupture 0.0765 GPa11.1 ksiGreen
 0.132 GPa19.2 ksi12% moisture content
Compressive Strength 5.58 MPa810 psiGreen, perpendicular to grain
 11.9 MPa1730 psi12% moisture content, perpendicular to grain
 30.9 MPa4480 psiGreen, parallel to grain
 61.6 MPa8940 psi12% moisture content, parallel to grain
Shear Strength 8.83 MPa1280 psiGreen, parallel to grain
 12.0 MPa1740 psi12% moisture content, parallel to grain
Impact 7777Impact bending in inches, 12% moisture content
 8888Impact bending in inches, green
Work to Maximum Load 0.156 J/cm³22.6 in-lb/in³12% moisture content
 0.180 J/cm³26.1 in-lb/in³Green
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.173 W/m-K1.20 BTU-in/hr-ft²-°FOven Dry, US origin
 0.202 W/m-K1.40 BTU-in/hr-ft²-°F12% Moisture Content, US origin
Shrinkage 7.7 %7.7 %Radial, from green to oven dry, US origin
 11 %11 %Tangential, from green to oven dry, US origin
 17.8 %17.8 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asian Mengkulang Wood
Honeylocust Wood
Japanese Oak Wood
Kauvula Wood
Laurel Red Oak Wood

PTSU023 / 71465

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.