MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Geniosil® XL 33 Silane
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Empirical formula: C8H16O5Si

CAS No.: 54586-78-6

Properties: Thanks to the increased rate of hydrolysis and condensation due to the alpha-effect, using GENIOSIL® XL 33 to modify the surface of inorganic fillers or pigments or in the production of moisture cured pipes and cables leads to substantially faster production processes and, in some cases, to greatly simplified treatment procedures (e.g. by making catalysts unnecessary). Used in plastics, fillers treated in this way exhibit improved dispersibility. Such mineral-filled plastics also show improved mechanical properties, while casting resins exhibit a pronounced reduction in melt viscosity. Use of GENIOSIL® XL 33 as a co-monomer in polymers results in binders that display extremely rapid curing and strong adhesion to the substrate thanks to the alpha-effect, and are additionally characterized by a pronounced improvement in wet scrub resistance and increased abrasion and scratch resistance. As a component of free-radical curable adhesives and sealants, GENIOSIL® XL 33 permits the adjustment of mechanical properties and results in improved substrate adhesion.

Special features: GENIOSIL® XL 33 is an alkoxysilane with a methacrylic organofunctional group. It´s a clear, colorless, light and heat sensitive liquid with a characteristically sweet odor. The silane hydrolyzes in the presence of moisture (methanol is released) to form silanols, which can then react with themselves to produce siloxanes.The close proximity of the alkoxysilyl group to the ester function results in greatly accelerated hydrolysis and condensation reactions (alpha-effect).As a bifunctional, organically unsaturated molecule, GENIOSIL® XL 33 can be incorporated into organic polymers, e.g. via radical grafting, and can simultaneously bond to inorganic substrates via the alkoxysilyl group. GENIOSIL® XL 33 can thus function as a molecular bridge between inorganic and organic substrates.

Application: GENIOSIL® XL 33 is mainly used as a surface modifier for glass fibers, fillers and pigments used in thermoplastics, thermosetting plastics and elastomers. As a polymer component of moisture-curing coatings or adhesive and sealant formulations, for example, GENIOSIL® XL 33 functions as a crosslinker and/or adhesion promoter. Other important uses are in the production of pipes and cables made of silanecrosslinked polyethylene (PE-Xb), in heat and/or radiation-curable adhesives and sealants and as an adhesion promoter in paints and industrial coatings.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.0721 g/cc
@Pressure 0.1013 MPa
DIN 51757
Molecular Weight 220.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 216.6 °C
@Pressure 0.1013 MPa
EU-GL.A.2
Flash Point 92.0 °CEN 22719
Ignition Temperature 295 °Cliquids; DIN 51794
 
Descriptive Properties
Content<30 mg/kgHydrolyzable chloride (as HCl)
Purity>96%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9335 / 204864

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.