MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Vibrantz Technologies EG 0002 Glazes and Sealants
Categories: Ceramic; Glass

Material Notes: Glass Type: Si-Al-Ba
Typical Powder Form: VWG
Typical Application: SiC

Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulating over glazes, binding agents and sealants for a variety of ceramic, metal, glass parts and substrates.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Particle Size 3.0 µm50% of particles
 <= 25 µm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.80 µm/m-°Cat Set Pt.
 3.20 µm/m-°C
@Temperature 260 °C
Softening Point >= 1000 °C
Annealing Point 845 °C
Transformation Temperature 825 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1300 °CTypical Firing Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vibrantz Technologies CF 7574 Glaze and Sealant Glass
Corning 1724 Aluminosilicate Crushed/Powdered Glass
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb
Titanium Carbide, TiC
Corning Large Cover Gorilla® Glass Touch Screen Glass

CFERR00 / 814

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.