MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex TEKRON® 4300-D88F Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes:

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 - 0.920 g/cc0.880 - 0.920 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inat 80°C for 30 min.
 0.0090 cm/cm0.0090 in/in
 0.012 cm/cm0.012 in/inat 93°C for 30 min.
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inat 80°C for 30 min.
 0.010 cm/cm0.010 in/in
 0.013 cm/cm0.013 in/inat 93°C for 30 min.
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 35 - 4035 - 4010 second delay; ASTM D2240
Tensile Strength, Yield 9.86 MPa1430 psiASTM D412
Elongation at Break 415 %415 %ASTM D412
Flexural Modulus 0.1500 GPa21.75 ksiASTM D790
 0.0620 GPa
@Temperature 70.0 °C
8.99 ksi
@Temperature 158 °F
ASTM D790
 2.079 GPa
@Temperature -30.0 °C
301.6 ksi
@Temperature -22.0 °F
ASTM D790
Instrumented Impact Energy at Peak  18.4 J
@Temperature 23.0 °C
13.6 ft-lb
@Temperature 73.4 °F
Multi-axial, at max. load
 22.4 J
@Temperature -40.0 °C
16.5 ft-lb
@Temperature -40.0 °F
Multiaxial, Peak Lead
Tear Strength 63.1 kN/m360 pliDie C; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
Flame Spread 25.4 mm/min1.00 in/minPass: Burn Rate- Max 100; FMVSS 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNO300 / 70043

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.