System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Americhem Engineered Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact
Categories:
Polymer
;
Thermoplastic
;
Acrylic (PMMA)
;
Acrylic, Impact Modified, Molded
Material Notes:
High impact version, extrusion or injection molding PMMA
All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.
Key Words:
PMMA
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.15
g/cc
ASTM D792
Linear Mold Shrinkage
0.0020
-
0.0060
in/in
0.125 in.; ASTM D955
Melt Flow
1.0
g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
45
ASTM D785
Tensile Strength, Yield
5500
psi
2.0 in/min; ASTM D638
Elongation at Break
35 %
2.0 in/min; ASTM D638
Elongation at Yield
5.0 %
2.0 in/min; ASTM D638
Flexural Strength
10000
psi
2.0 in/min; ASTM D790
Flexural Modulus
370000
psi
2.0 in/min; ASTM D790
Izod Impact, Notched
1.10
ft-lb/in
@Temperature 22.8 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
175
°F
Unannealed (0.250"); ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
410
-
450
°F
Middle Barrel Temperature
420
-
460
°F
Front Barrel Temperature
430
-
470
°F
Nozzle Temperature
420
-
460
°F
Melt Temperature
430
-
470
°F
Mold Temperature
150
-
190
°F
Drying Temperature
180
°F
Dry Time
3
-
4
hour
nominal; maximum drying time of 48 hours
Back Pressure
100
-
200
psi
Shot Size
40 - 60 %
Vent Depth
0.00100
-
0.00300
in
Screw Speed
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Americhem Engineered Compounds ColorFast® ACR100 Polymethylmethacrylate
LG Chemical HI835HS PMMA, Impact Resistant Grade
LG Chemical HI855HS PMMA, Impact Resistant Grade
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding
Lucite International Lucite® 4F Acrylic Bead Resin
PLTLC032 / 104417
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.