MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT ICM EM 1000SP Emulsion
Categories: Other Engineering Material

Material Notes: Description: This product is an industrial nonionic polydimethylsiloxane emulsion.

Key Features

  • High molecular weight
  • Mar resistance
  • Long lasting shine
  • Performs at low concentrations
Key Applications
  • Automotive Care
  • Rubber treatment
  • Mold release
  • Leather and Vinyl Care
Application: ICM EM-1,000SP is a 60% active emulsion of 1,000 cst polydimethylsiloxane. This non-ionic emulsion is specially developed to deliver the high molecular weight dimethicone actives in a low viscosity liquid with neutral pH. This emulsion is designed to be used as in mold release applications as well as a multi-substrate auto dressing and conditioner.

Addition Rates
Dosage – 1: 1-5%

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 8.08.0
Storage Temperature <= 40.0 °C<= 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Content0.6Silicone
IonicityNon-ionic
MIT FreeYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL288 / 314771

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.