MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco 800 NC Open Gear Lubricant
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubrication systems.

They provide a high film strength coating on gear teeth to minimize wear.

Chevron Open Gear Lubricants are designed to provide tacky, tenacious lubricant films on open gears operating under severe shock load conditions. Chevron Open Gear Lubricants contain a nonchlorinated diluent that eases the application of these lubricants onto the gears. The diluent then evaporates, leaving a tacky lubricant film on the gear teeth.

They can also be used to lubricate chains, sprockets, wire rope, and cables. When used as a cable coating, the diluent allows the lubricant to penetrate into the core, thus carrying the lubricant into the individual strands and minimizes wear as the cable is run through sheaves or onto a winch drum.

Applications

Chevron Open Gear Lubricants are recommended for all types of open gears, wire ropes, and cables. They can be applied by brush, swab, spray gun, or by automatic lubrication systems.

All grades provide lubrication for mining equipment including:

  • girth and pinion gears on rod and ball mills
  • rack and pinion gears on shovel dipsticks
  • and swing and pinion gears on top of the lower frame of shovels and draglines, which are sometimes served with an automatic lubrication system.
Chevron Open Gear Lubricants meet Bucyrus-Erie and P&H requirements for electric shovels and draglines.

Key Words: CPS Number: 255142; MSDS Number: 7088
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 38800 SUS
Saybolt Viscosity at 210°F 7320 SUS
Kinematic Viscosity at 40°C (104°F) 8375 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 1569 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kg
Four Ball Wear 0.570 mm
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Pour Point 10.0 °CASTM D97
Flash Point 88.0 °CASTM D92
 
Descriptive Properties
ColorBlack
Resultant FilmTacky
Rust Prevention, ASTM D665Pass
TextureSmooth

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV214 / 74829

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.