MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis PP4821 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: PP4821 is a thermoplastic, halogen-free, insulation compound based on a polypropylene copolymer. The composition of PP4821 is based on the elements Carbon and Hydrogen. Compounds based on these elements will therefore be the only significant constituents of the fumes due to the combustion of this product. Other elements may be present in concentrations less than 0.1%

Typical characteristics:

  • Superb system ageing compatibility
  • Processability on most PVC/PE extrusion equipment
  • Low water permeability
  • Pre-drying not required
Applications:
  • 70°C rated insulation for building wires (installation cables)
  • Power cables
  • Flexible cords
It can be used in areas sensitive to smoke or corrosive and toxic combustion products. PP4821 is stabilized for use in contact with copper.

Specifications: PP4821 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183-1
Melt Flow 3.10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48.0
@Time 15.0 sec
ISO 868
Tensile Strength 18.0 MPaISO 527
 >= 14.4 MPa
@Treatment Temp. 120 °C,
Time 1.21e+6 sec
After ageing; IEC 60811-401
Elongation at Break 600 %ISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 10.0 ohm-cmIEC 62631
Dielectric Constant 2.20
@Frequency 50 Hz
IEC 60250
Dielectric Strength >= 20.0 kV/mmIEC 60243
 
Processing PropertiesOriginal ValueComments
Zone 1 190 °C
Zone 2 200 °C
Zone 3 220 °C
Zone 4 220 °C
Die Temperature 220 °C
Drying Temperature 100 °C2 h in dehumidified air
Screw Speed 100 rpm
Shelf Life 24.0 Month
 
Descriptive Properties
Corrosivity of combustion fumes<10 µS/mmConductivity, IEC 60754-2
 >4.3 pHIEC 60754-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9871 / 323228

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.